Abstract
The authors regret that temperature-dependent yield strength of polyetheretherketone (PEEK) liners was not correctly defined as per the material properties listed in Table 3 during post-processing. As such, distribution of the through-laminate failure coefficient was not accurately displayed for high internal temperature (T0) load cases.